FIELD: methods for production of finely dispersed powders. SUBSTANCE: zirconium oxynitrate salt in the amount of 30.0 g is treated with solution of carbamide with concentration of 30 g/l and heated up to 90-100 C. Produced solution containing 206.0 g/l of zirconium is treated in plasma flux of plasma generator. Power consumption for production of 1 kg of zirconium dioxide amounts to 9.5 kWh. EFFECT: higher efficiency. 3 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS FOR PREPARING FINELY DISPERSIVE ZIRCONIUM DIOXIDE POWDER | 1993 |
|
RU2076069C1 |
METHOD OF PRODUCING URANIUM OXIDE FROM URANYL NITRATE SOLUTION AND DEVICE THEREFOR | 2015 |
|
RU2601765C1 |
METHOD USED FOR PRODUCTION OF THE METAL OXIDES POWDERS | 2006 |
|
RU2318723C2 |
METHOD OF URANYL NITRATE SOLUTION PROCESSING TO URANIUM OXIDE AND NITRIC ACID SOLUTION AND DEVICE FOR ITS IMPLEMENTATION | 2015 |
|
RU2599670C1 |
METHOD OF HIGH-CONCENTRATED URANIUM PROCESSING | 1997 |
|
RU2114061C1 |
METHOD OF PREPARING ULTRADISPERSE ELEMENT OXIDES | 1994 |
|
RU2073638C1 |
METHOD OF PRODUCTION OF HYDROFLUORIC ACID AND SILICON DIOXIDE | 2000 |
|
RU2175306C1 |
METHOD OF ZIRCONIUM HYDROXIDE PREPARING | 1991 |
|
RU2031845C1 |
COMPOSITE POWDER BASED ON DOPED TITANIUM CARBONITRIDE | 2024 |
|
RU2823899C1 |
METHOD OF PRODUCING TITANIUM NITRIDE NANOPOWDERS | 2010 |
|
RU2434716C2 |
Authors
Dates
1995-02-09—Published
1990-07-09—Filed