FIELD: fireproof and thermoresistant foam plastics. SUBSTANCE: simple polyesters of different molecular mass were mixed with antipyrene, frothing agent of surface-active substance, polyisocyanate and catalytic mixture consisting of Lewis base and potassium dimethylaminopropionate taken at the ratio (0.25-7): 1, respectively. Composition is poured into the closed form and kept for 20 min. Prepared samples show apparent density 55.8-49.7 kg/m3, compression strength 292-394 kPa, stretching strength 204-350 kPa. EFFECT: improved method of foam plastic production. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF HARD POLYURETHANE FOAM | 1990 |
|
SU1832694A1 |
METHOD OF PREPARING RIGID THERMOSHAPED POLYURETHANE FOAM | 1991 |
|
SU1824877A1 |
METHOD FOR PRODUCTION OF ISOCYANURATE-CONTAINING FOAM PLASTIC | 1989 |
|
SU1811183A1 |
METHOD OF POLYURETHANE ISOCYANURATE FOAM PREPARING | 1987 |
|
RU1612559C |
PROCESS FOR PREPARING POLYISOCYANURATE-CONTAINING PLASTIC FOAM | 1988 |
|
SU1818829A1 |
PROCESS FOR PREPARING RIGID POLYURETHANE FOAM OR POLYISOCYANURATE FOAM | 1993 |
|
RU2048482C1 |
CATALYST FOR MANUFACTURING FOAMED POLYURETHANE AND METHOD OF ITS PRODUCTION | 1986 |
|
RU1513884C |
CATALYST FOR PRODUCING FOAMED POLYURETHANES AND FOAMED POLYISOCYANURATES | 1986 |
|
RU1438197C |
METHOD OF POLYURETHANE FOAM PREPARING | 1986 |
|
RU1635519C |
METHOD OF PRODUCING ISCCYANURATE CONTAINING FOAMED PLASTICS | 0 |
|
SU472558A1 |
Authors
Dates
1996-04-10—Published
1991-12-04—Filed