FIELD: organic chemistry. SUBSTANCE: polyether or mixture of polyethers are mixed with fireproofing compound, surfactant and with frothing agent. Polyisocyanate and catalytic mixture of tertiary amine and potassium dimethylamino propionate (their molar ratio being 30-2:1) are added. Compressive strength of the samples is 318-424 kPa, bending strength is 439-698 kPa. EFFECT: improves efficiency of method. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ISOCYANOURATE-CONTAINING FOAM PLASTIC PRODUCING | 1991 |
|
SU1826493A1 |
METHOD OF PREPARING RIGID THERMOSHAPED POLYURETHANE FOAM | 1991 |
|
SU1824877A1 |
PROCESS FOR PREPARING RIGID POLYURETHANE FOAM OR POLYISOCYANURATE FOAM | 1993 |
|
RU2048482C1 |
PROCESS FOR PREPARING POLYISOCYANURATE-CONTAINING PLASTIC FOAM | 1988 |
|
SU1818829A1 |
METHOD OF PREPARING RIGID POLYURETHANE FOAM FOR CAR DOOR UPHOLSTERING | 1990 |
|
SU1832693A1 |
RIGID POLYURETHANE FOAM MANUFACTURE PROCESS | 2003 |
|
RU2280046C2 |
COMPOSITION FOR PREPARING ELASTIC POLYURETHANE FOAM BY MOLDING METHOD | 1998 |
|
RU2142968C1 |
METHOD OF PREPARING OF INFLEXIBLE POLYURETHANE FOAM | 1991 |
|
RU2028316C1 |
METHOD OF POLYURETHANE FOAM PREPARING | 1986 |
|
RU1635519C |
COMPOSITION FOR PRODUCTION OF SPRAYED HARD POLYURETHANE FOAMS | 2007 |
|
RU2350629C1 |
Authors
Dates
1996-02-27—Published
1990-12-04—Filed