FIELD: manufacture of sealants, coatings and foundry products. SUBSTANCE: when preparing elastomers, the product of reaction of liquid oligomers having reactive groups and a diisocyanate in a 1.0: (3.4-4.0) molar ratio respectively is treated with a mixture of a liquid diene oligomers having end hydrozide or hydrazone groups and an aromatic diamine in a (0.2-1.0): (1.2-2. ) molar ratio respectively. The curing operation is accomplished in a mold 20-2 C for 21 hr. EFFECT: improved quality of elastomers. 12 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR PREPARING ELASTOMERS | 1982 |
|
RU2005750C1 |
COMPOSITION FOR PREPARING COATINGS | 0 |
|
SU1789541A1 |
OLIGODIENENMIDOURETHANE DIISOCYANATES FOR MANUFACTURING SEALING COMPOSITIONS, FOUNDRY PRODUCTS AND CHEMICALLY RESISTANT COATINGS | 1992 |
|
RU2005736C1 |
POLYURETHANE COMPOSITION | 1998 |
|
RU2155781C2 |
PROCESS FOR PREPARING ELASTOMERS BASED ON OLIGOBUTADIENE DIHYDRAZONE OR OLIGOISOPRENE DIHYDRAZONE | 1989 |
|
RU2076878C1 |
LIQUID PREPOLYMER HARDENER WHICH HAS TERMINAL ISOCYANATE GROUPS | 2016 |
|
RU2633520C1 |
POLYURETHANE COMPOSITE | 2000 |
|
RU2186803C2 |
LIQUID HARDENING AGENT FOR POLYURETHANE SYSTEMS | 2005 |
|
RU2292358C1 |
LIQUID PREPOLYMER HARDENER WITH END ISOCYANATE GROUPS | 1996 |
|
RU2122006C1 |
METHOD OF GETTING A POLYMER-BITUMEN BENDING BASED ON FOAMED POLYURETHANE | 2017 |
|
RU2648097C1 |
Authors
Dates
1994-01-15—Published
1992-07-16—Filed