FIELD: polymeric materials. SUBSTANCE: method involves mixing of 5-60 mas. p. waste of polycaproamide or propylene fibers together with 40-95 mas. p. waste of polyacrylonitrile fibers (length is 2-20 mm) and pressing under pressure 30-60 kgf/30-60 kgs/cm2 for 1-1.5 min/mm material thickness, at 160-190 C for press-material with polypropylene fibers and at 190-210 C for press-material with polycaproamide fibers. EFFECT: improved method of material producing. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PLATE MATERIAL | 1994 |
|
RU2103165C1 |
MEANS FOR PROTECTING FROM LOW TEMPERATURE | 1991 |
|
RU2009650C1 |
METHOD FOR PRODUCTION OF NONWOVEN BONDED MATERIAL | 1991 |
|
RU2057217C1 |
METHOD OF EVALUATION OF STRAIGHTENING OF FIBRES | 1992 |
|
RU2027992C1 |
COMPOSITION FOR PREPARING RELIEF PICTURE ON TEXTILE MATERIALS OF NATURE OR CHEMICAL FIBERS | 1990 |
|
RU2012701C1 |
METHOD OF MEASUREMENT OF TEMPERATURE OF OBJECT | 1991 |
|
RU2036443C1 |
METHOD OF FIBROUS MATERIAL MAKING | 1991 |
|
RU2005828C1 |
METHOD FOR DETERMINING BRITTLENESS OF LENGTHY MATERIALS | 1991 |
|
RU2009487C1 |
METHOD OF DETERMINING ELECTRIC-PHYSICAL PARAMETERS OF DIELECTRICS BY DISCHARGE | 1991 |
|
RU2007737C1 |
FIBER MATERIAL MOLDING DEVICE | 1991 |
|
RU2026905C1 |
Authors
Dates
1994-05-15—Published
1991-01-02—Filed