FIELD: electronics. SUBSTANCE: mixture of starting wolfram powder with scandium oxide is oxidized in the air at 400-700 C and is reduced in atmosphere of hydrogen at 1000-1300 C and after this is impregnated with barium-calcium aluminate. EFFECT: facilitated manufacture, improved operational characteristics. 2 dwg
Title | Year | Author | Number |
---|---|---|---|
METAL CATHODE AND ITS MANUFACTURING PROCESS | 2000 |
|
RU2172997C1 |
METHOD FOR MANUFACTURING POROUS-METAL CATHODES FROM TUNGSTEN POWDER | 2005 |
|
RU2297068C2 |
METHOD FOR MANUFACTURING METAL-POROUS CATHODES FROM TUNGSTEN POWDER | 2005 |
|
RU2293395C1 |
METHOD FOR PRODUCING POROUS-METAL CATHODES FROM TUNGSTEN POWDER | 2005 |
|
RU2293394C1 |
TWO-LAYER DISPENSED CATHODE AND METHOD OF ITS MANUFACTURING | 2019 |
|
RU2724980C1 |
0 |
|
SU201549A1 | |
METHOD FOR PRODUCING METAL POROUS CATHODE | 2014 |
|
RU2583161C1 |
TARGET FOR DISPENSER CATHODE BASED ON BARIUM SCANDE | 2012 |
|
RU2624264C2 |
DISPENSER SOAKED CATHODE FOR MAGNETRON | 2007 |
|
RU2342732C1 |
METHOD OF MAKING METAL-POROUS CATHODE | 2023 |
|
RU2823125C1 |
Authors
Dates
1994-05-15—Published
1991-04-17—Filed