FIELD: metal working. SUBSTANCE: method comprises two stages of chilling and tempering; carrying out first chilling stage from temperature, being by 90 ± 3 C higher, than temperature of α-γ transition; heating for second stage of chilling with a rate, consisting 33-35 C/min and more till temperature value, being by (70 ± 3)C higher, than temperature of α → γ transition. EFFECT: enhanced quality of treated steels. 1 cl
Title | Year | Author | Number |
---|---|---|---|
PEARLITE CLASS LOW-ALLOYED HYPEREUTECTOID STEELS PROCESSING METHOD | 1992 |
|
RU2048540C1 |
METHOD TO CONTROL FRICTION WELDING PROCESS | 1991 |
|
RU2009818C1 |
METHOD FOR HEAT TREATMENT OF STEEL | 1992 |
|
RU2044070C1 |
TOOL STEELS THERMAL PROCESSING METHOD | 1991 |
|
RU2017838C1 |
METHOD OF THERMAL TREATMENT OF ARTICLES OF STEELS OF PERLITE CLASS | 0 |
|
SU1611951A1 |
THERMOMECHANICAL PROCESSING OF LIGHTLY-ALLOYED STEELS | 2013 |
|
RU2548339C1 |
METHOD OF HEAT TREATMENT OF STEEL PARTS | 2022 |
|
RU2800483C1 |
MULTILAYER ARMORED BARRIER (VERSIONS) | 2008 |
|
RU2388986C2 |
METHOD FOR VACUUM HEAT TREATMENT OF SHAPE-FORMING TOOLS | 1992 |
|
RU2031147C1 |
METHOD FOR MACHINING QUICK-CUTTING STEEL | 1988 |
|
RU2024631C1 |
Authors
Dates
1994-07-15—Published
1991-11-25—Filed