FIELD: chemical industry. SUBSTANCE: the frit of a ground-coat sheet-steel enamel comprises (wt %): 34-37 silicon oxide SiO2; 4-6 aluminium oxide; 18-22 boron oxide; 23-25.5 sodium oxide; 1.4-2.5 titanium oxide; 1.9-2.3 phosphorus oxide; 4.3-5.0 ferric oxide; 1.4-1.6 cobalt oxide; 5-6 manganese oxide; 0.7-0.9 nickel oxide, the Co2O3 to Ni2O3 ratio being 1.77-2.0. The characteristic of the ground-coat enamel: the firing range 320-330 C and the impact strength 11.76-14.99 kgm/J. EFFECT: improved properties of the ground-coat enamel. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ENAMEL FOR STEEL | 1992 |
|
RU2016862C1 |
ENAMEL | 1993 |
|
RU2041174C1 |
SILICATE ENAMEL COATING FOR INTERNAL PROTECTION OF STEEL PIPELINES | 2020 |
|
RU2769688C2 |
ENAMEL "STAVAN" | 2001 |
|
RU2203234C2 |
ENAMEL SLIP FOR GROUNDING COAT | 1998 |
|
RU2148557C1 |
METHOD OF PREPARING ENAMEL COATING | 1998 |
|
RU2154036C2 |
PRIMER ENAMEL FRIT FOR APPLYING BY ELECTROSTATIC METHOD | 1994 |
|
RU2127710C1 |
FRIT FOR DIRECT-ON ENAMEL | 1992 |
|
RU2036174C1 |
HEAT-RESISTANT MULTIFUNCTIONAL COATING | 2023 |
|
RU2812460C1 |
ENAMEL FRIT COMPOSITION | 1991 |
|
RU2008283C1 |
Authors
Dates
1994-09-30—Published
1990-12-25—Filed