FIELD: metallurgy, production of items for operation in aggressive media at high loads. SUBSTANCE: ferritic steel workpiece is annealed at 475 C temper brittleness drawing temperature within from 1.5 to 2 h, forged at increased strain temperature within from 450 - 500 to 640 - 650 C with total strain amounted for 150 to 200 per cent. Then it is thermally treated within 565 to 580 C temperature and water cooled. EFFECT: almost full recrystallization with 1 to 3 microns medium grain size. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
STEEL TREATMENT METHOD | 2000 |
|
RU2181776C2 |
METHOD FOR MACHINING OF AUSTENITIC-MARTENSITIC STEELS | 0 |
|
SU1735390A1 |
METHOD OF PROCESSING THE BLANKS FROM γ+α HYPEREUTECTOID ALLOYS | 1999 |
|
RU2164263C2 |
METHOD OF TREATMENT OF CAST HYPEREUTECTOID ALLOYS ON BASE OF TITANIUM ALUMINIDES γ-TiAl AND αTlAl | 2001 |
|
RU2203976C2 |
METHOD OF DIFFUSION WELDING OF TWO-PHASE TITANIUM ALLOYS | 1991 |
|
RU2025240C1 |
PROCESS FOR ROLLING BILLETS OF HYPEREUTECTOID γ+α-ALLOYS AND METHOD FOR MAKING BILLETS FOR SUCH PROCESS | 1999 |
|
RU2164180C2 |
METHOD FOR MAKING WHEELS OF TRANSPORT VEHICLES | 1998 |
|
RU2153946C2 |
METHOD FOR WORKING BLANKS OF METALS AND ALLOYS | 1998 |
|
RU2159162C2 |
METHOD OF WORKING, MAINLY, LARGE-SIZED BLANKS FROM (ALPHA+BETTA)-TITANIUM ALLOYS | 2001 |
|
RU2196189C2 |
METHOD FOR MAKING PISTON OF INTERNAL COMBUSTION ENGINE | 1999 |
|
RU2176943C2 |
Authors
Dates
1994-11-15—Published
1991-04-29—Filed