FIELD: pressure welding. SUBSTANCE: method comprises steps of deforming a blank of two-phase titanium alloy with grain size (0.3-0.5) micrometers at temperature (400-550)C with a rate 10-5... 10-2s-1 according to omnidirectional forging pattern up to a total forging degree (80-300)%; preparing a surface of the blank and performing a diffusion welding process at temperature, equal to 200-400 C. EFFECT: enhanced quality of welded products. 1 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR OBTAINING SEMI-FINISHED PRODUCTS FROM METALS AND ALLOYS BY PSEUDOPOWDER METALLURGY PROCESS | 2001 |
|
RU2208063C2 |
METHOD OF PROCESSING THE BLANKS FROM γ+α HYPEREUTECTOID ALLOYS | 1999 |
|
RU2164263C2 |
PROCESS FOR ROLLING BILLETS OF HYPEREUTECTOID γ+α-ALLOYS AND METHOD FOR MAKING BILLETS FOR SUCH PROCESS | 1999 |
|
RU2164180C2 |
METHOD OF WORKING, MAINLY, LARGE-SIZED BLANKS FROM (ALPHA+BETTA)-TITANIUM ALLOYS | 2001 |
|
RU2196189C2 |
METHOD OF TREATMENT OF BLANKS MADE FROM METALS OR ALLOYS | 2000 |
|
RU2203975C2 |
METHOD FOR WORKING BLANKS OF METALS AND ALLOYS | 1998 |
|
RU2159162C2 |
METHOD OF TREATMENT OF CAST HYPEREUTECTOID ALLOYS ON BASE OF TITANIUM ALUMINIDES γ-TiAl AND αTlAl | 2001 |
|
RU2203976C2 |
METHOD TO PRODUCE METAL PROTECTIVE PATCH PIECE | 2014 |
|
RU2553759C1 |
METHOD FOR MANUFACTURING OF SEMI-FINISHED SHEET PRODUCT FROM TITANIUM ALLOY | 2006 |
|
RU2320771C1 |
METHOD FOR TREATING NICKEL-BASE DISPERSION-HARDENED ALLOYS | 1992 |
|
RU2041284C1 |
Authors
Dates
1994-12-30—Published
1991-04-30—Filed