FIELD: chemical technology. SUBSTANCE: granules of activated carbon are impregnated with 0.15-0.35 wt.-% aqueous solution of silver nitrate at 30-50 C for 10-15 min and dried by gas-air mixture at 150-200 C. EFFECT: improved method of activated carbon preparing. 2 cl, 1 tbl