FIELD: production of inorganic sorbents. SUBSTANCE: sorbent is produced by electrochemical dissolving of aluminium in 0.5-3.0 M solution of lithium chloride at current density of 8-20 A/sq.dm for 1-2 h. Produced precipitate is separated by filtering. Sorbent is prepared for sorption process by its treatment with water with intensive stirring to remove a portion of lithium from sorbent matrix. EFFECT: higher efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING GRANULAR SORBENT FOR EXTRACTING LITHIUM FROM LITHIUM-CONTAINING BRINE | 2010 |
|
RU2455063C2 |
METHOD OF PRODUCING LITHIUM HYDROXIDE FROM BRINES AND PLANT FOR METHOD EMBODIMENT | 1998 |
|
RU2193008C2 |
METHOD TO PRODUCE GRANULATED SORBENT FOR LITHIUM EXTRACTION FROM BRINES | 1993 |
|
RU2050184C1 |
METHOD OF PRODUCTION OF A SORBENT FOR EXTRACTION OF LITHIUM FROM SALINE SOLUTIONS | 2002 |
|
RU2234367C1 |
METHOD FOR OBTAINING GRANULAR SORBENT FOR EXTRACTION OF LITHIUM FROM LITHIUM-CONTAINING BRINES | 2021 |
|
RU2804183C1 |
METHOD AND APPARATUS OF SELECTIVE SORPTION EXTRACTION OF LITHIUM FROM BRINES | 1993 |
|
RU2050330C1 |
SORBENT FOR EXTRACTING LITHIUM FROM LITHIUM-CONTAINING SOLUTIONS, ITS USE FOR EXTRACTING LITHIUM FROM LITHIUM-CONTAINING SOLUTIONS AND METHOD OF PRODUCING SUCH SORBENT | 2023 |
|
RU2816101C1 |
METHOD OF PREPARING LITHIUM-CONTAINING FLUORIDE SALTS FOR ELECTROLYTIC ALUMINUM PRODUCTION | 1999 |
|
RU2184704C2 |
METHOD OF PREPARING LITHIUM ALUMINATE | 1997 |
|
RU2113405C1 |
METHOD OF PREPARING SORBENT FOR RECOVERING LITHIUM FROM BRINES | 2001 |
|
RU2223142C2 |
Authors
Dates
1995-02-09—Published
1992-05-25—Filed