FIELD: mechanical engineering. SUBSTANCE: method is realized with use of powerful energy source - gas-flame jet directed at angle of 34-37 deg. to work surface. Used for cutters are steels capable of hardening in the air mainly, silicon-manganese steels. Simultaneously, cutter edges are formed, sharpened and thermally hardened. EFFECT: higher efficiency, involving no complicated processes or specific regulation of temperature or other parameters of process. 2 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR STRENGTHENING CUTTING EDGES OF COUNTER-CUTTING PLATE OF AGRICULTURAL MACHINE | 2009 |
|
RU2410211C1 |
METHOD FOR HARDENING THE SHEAR PLATE OF A MULCHING CUTTER | 2022 |
|
RU2799598C1 |
METHOD OF MAKING KNIVES | 0 |
|
SU623886A1 |
METHOD FOR LASER HARDENING OF WORKING SURFACES OF CUTTING TOOL EDGE | 2021 |
|
RU2781887C1 |
METHOD OF TEMPERING PARTS FROM LOW-CARBON BORON-CONTAINING STEEL | 2018 |
|
RU2690386C1 |
PRODUCTION TILLAGE TOOL WORKING MEMBERS | 2013 |
|
RU2528687C1 |
METHOD FOR OBTAINING WEAR-RESISTANT AND ELASTIC STRUCTURES OF REPLACEABLE BODIES OF SOIL CULTIVATION EQUIPMENT | 2020 |
|
RU2769338C2 |
METHOD OF WELDED CUTTING TOOL HEAT TREATMENT | 0 |
|
SU1770403A1 |
METHOD OF SAW STRENGTHENING | 2006 |
|
RU2333971C2 |
SELF-SHARPENING CUTTING TOOL WITH HARD COATING | 2003 |
|
RU2305623C2 |
Authors
Dates
1995-03-20—Published
1992-07-09—Filed