FIELD: leather tanning. SUBSTANCE: pickled depilated hide after preliminary chrome tanning is tanned with composition containing, wt.-%: chrome tanning agent 23-35; neutralizing agents 30-40; waste in adipic acid production 3-33; polymethylenenaphthalene sodium sulfonate 2-16; lignosulfonate sodium 2-16. Firstly tanning is carried out at 20-25 C at composition consumption 1.0-1.5% of hide mass for 1-2 h, and then at 30-35 C at composition consumption 2.0-3.5% of hide mass for 4-6 h. EFFECT: improved method of leather tanning. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR LEATHER TANNING | 1993 |
|
RU2031956C1 |
COMPOSITION FOR LEATHER TANNING | 1993 |
|
RU2031955C1 |
PROCESS FOR FINISHING LEATHER | 1993 |
|
RU2043421C1 |
PROCESS FOR FINISHING LEATHER | 1993 |
|
RU2043420C1 |
METHOD FOR TREATMENT OF LEATHER | 1993 |
|
RU2039086C1 |
METHOD FOR PREPARING SPLIT OF FLESH SIDE OF HIDE | 1992 |
|
RU2036972C1 |
PROCESS FOR MAKING TANNED PELT | 1991 |
|
RU2005792C1 |
METHOD OF WORKING OUT TANNED INTERMEDIATE PRODUCT | 1997 |
|
RU2107731C1 |
METHOD OF MANUFACTURING LEATHER WITH TIGHTENED FACE SURFACE | 1999 |
|
RU2157410C1 |
METHOD OF LEATHER OUTPUT | 1991 |
|
RU2030456C1 |
Authors
Dates
1995-03-27—Published
1993-04-13—Filed