FIELD: building materials production. SUBSTANCE: proposed composition contains (mass % ): furfural-acetone resin 15.0-25.0, benzenesulfonic acid 3.0-5.0, andezite flour 47.0-57.0, technical carbon black 2.6-5.7, ground glass 0.3-0.5, wood chips 16.0-20.0. Bending strength thus prepared material is 19-29 MPa, its elasticity modulus being 1.30-1,30...1,64·104 MPa. EFFECT: improves operating properties. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR COMPOSITE MATERIAL | 1995 |
|
RU2098375C1 |
BUILDING MEMBER | 1992 |
|
RU2032783C1 |
COMPOSITE FOR COMPOSITION MATERIAL | 2001 |
|
RU2215705C2 |
POLYMER COMPOSITION | 2000 |
|
RU2198190C2 |
COMPOSITION FOR WOOD-POLYMER COMPOSITE MATERIAL | 2009 |
|
RU2405010C2 |
COMPOSITION FOR WOOD-POLYMER COMPOSITE MATERIAL | 2011 |
|
RU2543870C2 |
CONSTRUCTION MEMBER | 1997 |
|
RU2117119C1 |
METHOD FOR OBTAINING HEAT-INSULATING MATERIAL, BASED ON WOOD AND THERMOPLASTIC WASTES | 2014 |
|
RU2581047C2 |
EPOXY BINDER FOR COMPOSITE MATERIALS | 2021 |
|
RU2788335C1 |
MOLDED MATERIAL, METHOD OF ITS PRODUCTION AND METHOD OF PRODUCING COMPOSITE MATERIAL BASED ON MOLDED MATERIAL | 1999 |
|
RU2152966C1 |
Authors
Dates
1995-04-10—Published
1992-03-24—Filed