FIELD: aerospace engineering. SUBSTANCE: solution or aqueous emulsion of polymethylsiloxane oligomer having structural formula , ratio CH3/Si = 1,66 being 1.66 is applied on the surface of heat insulating material. Said material is allowed to stand within 60-70 min on open air, then heat treatment within 1.5-2 h at 200-400 C is carried out. Water absorption by immersion within 24 h is 2.0-6.2 %. EFFECT: improves efficiency of the method. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF HYDROPHOBIZING POROUS HEAT-SHIELDING MATERIALS | 1983 |
|
RU2068830C1 |
RELEASE COATING (VERSIONS) | 1997 |
|
RU2122561C1 |
ANTIADHESIVE COATING | 1992 |
|
RU2034887C1 |
HEAT-SHIELDING POLYMERIC MATERIAL AND METHOD FOR ITS PREPARING | 2001 |
|
RU2220169C2 |
METHOD OF PREPARING OF ADDITIVE AGENT TO POLYORGANOSILOXANES | 1992 |
|
RU2034868C1 |
HEAT-STABLE GLUE COMPOSITION | 1991 |
|
RU2021314C1 |
METHOD OF MANUFACTURING HIGH-TEMPERATURE ALUMINA-BASED FIBER | 2001 |
|
RU2212388C2 |
POLYMER SOUND-ABSORBING MATERIAL AND METHOD FOR ITS MANUFACTURING | 2015 |
|
RU2612674C1 |
GLUE COMPOSITION FOR TENSORESISTOR GLUEING | 1990 |
|
RU1818832C |
METHOD OF MANUFACTURING ABRADABLE MATERIAL | 1993 |
|
RU2039631C1 |
Authors
Dates
1995-04-10—Published
1982-05-26—Filed