FIELD: leather industry. SUBSTANCE: depilated hide flesh side of hide split is pickled with sulfuric acid, sodium chloride and ammonium sulfate at their consumption, 0.2-0.3; 1.5-2.5 and 3.5-4.5 of hide mass, respectively, following by tanning, shaving, additional tanning with chromed and synthetic tanning agents, neutralization, greasing in the presence of sodium hydrocarbonate and ammonium aqueous solution at their consumption 1.5-2.0% and 1.0-1.5% respectively, of shaved split following by drying, polishing, soaking, staining, greasing, treatment with acetic acid for two stages with intermediate washing and the terminal finishing. EFFECT: improved method of velour production. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF LEATHER PRODUCTION FOR SHOES UPPER PART FROM THE SPLIT | 1993 |
|
RU2039834C1 |
METHOD OF LEATHER PRODUCTION | 1993 |
|
RU2039833C1 |
METHOD OF PRODUCTION OF FLEECY LEATHER, MAINLY BUFFED-GRAIN LEATHER | 1993 |
|
RU2039837C1 |
METHOD OF HYDROPHOBIC LEATHER PRODUCTION | 1993 |
|
RU2039835C1 |
METHOD FOR PREPARING SPLIT OF FLESH SIDE OF HIDE | 1992 |
|
RU2036972C1 |
METHOD OF MANUFACTURING VELOURS FROM SPLIT | 2003 |
|
RU2225449C1 |
METHOD OF LEATHER MAKING | 1996 |
|
RU2096474C1 |
METHOD OF PRODUCING HIDES WITH A COAT OF HAIR | 0 |
|
SU1221254A1 |
CORIUM OF GENUINE LEATHER AND FUR SEMIFINISHED PRODUCT AND METHODS FOR MANUFACTURE THEREOF | 2002 |
|
RU2206620C1 |
METHOD FOR ELASTIC LEATHERS PRODUCTION | 0 |
|
SU1730172A1 |
Authors
Dates
1995-07-20—Published
1993-12-10—Filed