FIELD: organoelement chemistry. SUBSTANCE: dialkylmonotellurides were synthesized by tellurium cathode dissolving in alkaline heterophase electrolyte at the current density 0,1-0,2 A/sm2, at voltage 180-250 V in the presence of polarizing addition at dielectric constant value 20, not less. EFFECT: improved method of synthesis.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF GERMANIUM HYDRIDE PRODUCING | 1992 |
|
RU2071993C1 |
METHOD OF SYNTHESIS OF GERMANIUM HYDRIDE | 1990 |
|
SU1732697A1 |
METHOD OF ELECTROCHEMICAL OBTAINING OF ALUMINUM OXIDE POWDERS | 2017 |
|
RU2664135C1 |
METHOD OF PRODUCING NIOBIUM METHYLATE | 2007 |
|
RU2371428C2 |
PROCEDURE FOR PRODUCTION OF POWDERS OF HIGH-MELTING METALS | 2009 |
|
RU2397279C1 |
METHOD OF SYNTHESIS OF PHOSPHORIC ACID ESTERS | 2001 |
|
RU2199545C1 |
METHOD FOR PREPARING HALOGENATED PARAFFIN BASED ON HIGHER ALPHA-OLEFINS | 2005 |
|
RU2288908C1 |
METHOD OF DETERMINATION OF GAS-FORMING IMPURITIES IN SOLID HIGHLY PURE SUBSTANCES | 1995 |
|
RU2089884C1 |
METHOD OF PRODUCING HYDROGEN SELENIDE | 0 |
|
SU1673642A1 |
METHOD FOR SEPARATION OF BISMUTH FROM LEAD | 1992 |
|
RU2049158C1 |
Authors
Dates
1995-08-09—Published
1992-11-10—Filed