FIELD: metallurgy. SUBSTANCE: burden has by weight: alloyed (carbonaceous) wastes 10-55, metallized concentrate of siderite 15-30, metal-abrasive wastes 30-60, with ratio of metallized concentrate and metal-abrasive wastes being 1:(1-3). EFFECT: increased efficiency by improved extraction of alloying components from metal-abrasive wastes, reduced consumption of burden. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF REMELTING LIGHT-WEIGHT METAL CHARGE | 0 |
|
SU655727A1 |
METHOD OF MELTING VANADIUM-CONTAINING STEEL IN ELECTRIC ARC FURNACE | 1996 |
|
RU2102497C1 |
METHOD OF MAKING STEEL IN HIGH-POWER ELECTRIC ARC FURNACES | 2000 |
|
RU2201970C2 |
METHOD OF MAKING HIGH-ALLOY STEEL | 2003 |
|
RU2255983C1 |
METHOD OF PREPARING NICKEL-CONTAINING ADDITION ALLOY | 1996 |
|
RU2095427C1 |
METHOD OF SMELTING LOW-CARBON STEELS | 1996 |
|
RU2103379C1 |
METHOD FOR MELTING LOW-CARWON CORRER-CONTAINING HIGH-CHROMIUM STEELS | 0 |
|
SU956574A1 |
METHOD FOR MELTING NATURALLY ALLOYED STEELS AND ALLOYS IN HEARTH FURNACES | 1994 |
|
RU2113496C1 |
METHOD OF PREPARATION OF ELECTRIC FURNACE FOR PRODUCTION OF SYNTHETIC SLAG | 1994 |
|
RU2082764C1 |
METHOD OF MELTING OF CARBONIC AND LOW ALLOYED GRADES OF STEEL | 2006 |
|
RU2336310C2 |
Authors
Dates
1995-08-27—Published
1993-02-17—Filed