FIELD: engineering and medicine. SUBSTANCE: 0.1-0.9 wt part per 1 wt part of a ultraphosphate and an organic polymer are charged into an extruder and stirred at 180-300 C. The melt is then extruded or pressed. EFFECT: more efficient preparation process. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD FOR PRODUCING THREE-DIMENSIONAL PRODUCTS OF COMPLEX SHAPE WITH NATIVE TRABECULAR BONE STRUCTURE BASED ON HIGH-VISCOSITY POLYMER | 2019 |
|
RU2708589C1 |
| METHOD OF OBTAINING POLYMERIC COATING ON SURFACE OF BUILDING PRODUCTS | 1992 |
|
RU2046719C1 |
| GLASS | 1991 |
|
RU2017708C1 |
| MATERIAL FOR PROTECTIVE COATINGS OF BUILDING STRUCTURES AND METHOD OF PREPARATION THEREOF | 1996 |
|
RU2129133C1 |
| PRODUCTION OF ARTICLES FROM GRANULATED POLYMER MATERIALS (VERSIONS) | 2012 |
|
RU2527049C2 |
| LUBRICANT COMPOSITION | 2015 |
|
RU2596820C1 |
| COMPOSITION AND DOSAGE FORM CONTAINING SOLID OR SEMISOLID MATRIX | 2006 |
|
RU2423997C9 |
| METHOD OF PRODUCING BITUMEN POLYMER MATERIALS | 2011 |
|
RU2468050C1 |
| METHOD FOR PRODUCTION OF FOAMED POLYVINYLCHLORIDE MATERIAL (VERSIONS) | 1993 |
|
RU2045549C1 |
| COMPOSITE FILLER FOR POLYMERS BASED ON PHOSPHOGYPSUM | 2023 |
|
RU2812080C1 |
Authors
Dates
1995-11-20—Published
1992-02-14—Filed