FIELD: oil mechanical engineering. SUBSTANCE: after heading of rod heads it is heated up to 500 600 C, held under that temperature for definite time and cooled in the open air. Rods are subjected to straightening and finishing machining. In the case straightening is exercised either with additional heating up to 500 700 C or after heading of rod heads, or right after holding under temperature of 500 700 C. EFFECT: improved process of pump rods production. 4 cl, 3 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PUMP ROD MANUFACTURE METHOD | 1992 |
|
RU2048546C1 |
METHOD OF TESTING SUCKER RODS AT STRAIGHTENING THEM | 1993 |
|
RU2076008C1 |
METHOD OF STRAIGHTENING PUMP RODS | 1994 |
|
RU2069113C1 |
METHOD OF SUCKER RODS STRINGS ASSEMBLY AND SUCKER RODS STRING STAGE | 1994 |
|
RU2068484C1 |
METHOD OF MANUFACTURING PUMP RODS | 1994 |
|
RU2069119C1 |
MANUFACTURING METHOD OF PUMPING ROD | 2006 |
|
RU2340683C2 |
HOLLOW PUMP ROD | 2007 |
|
RU2371565C2 |
METHOD OF PRODUCTION OF THE PETROLEUM PUMPING RODS | 2005 |
|
RU2270871C1 |
METHOD FOR MAKING HEAT HARDENED BLANKS OF PUMP RODS | 1997 |
|
RU2117539C1 |
METHOD OF MAKING PUMP RODS | 1997 |
|
RU2119858C1 |
Authors
Dates
1995-11-20—Published
1992-03-31—Filed