FIELD: radioelectronic industry. SUBSTANCE: flux for tinning resistor leads has the following components, mas.%: glycerin 30-55; surfactant 7-12; aniline hydrochloride 6-15; the balance, dihydric alcohol. Dihydric alcohol is used in form of ethylene glycol or polyethylene glycol. EFFECT: higher efficiency. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR TINNING OF RADIO ELEMENTS TERMINALS | 2009 |
|
RU2386521C1 |
METHOD OF TINNING LEADS OF RADIO COMPONENTS | 0 |
|
SU1555074A1 |
FLUX FOR LOW-TEMPERATURE SOLDERING | 2010 |
|
RU2463145C2 |
FLUX FOR LOW-TEMPERATURE SOLDERING OF COPPER AND NICKEL | 0 |
|
SU1459874A1 |
FLUX FOR LOW-TEMPERATURE SOLDERING | 2010 |
|
RU2463144C2 |
FLUX FOR LOW-TEMPERATURE SOLDERING | 2010 |
|
RU2463143C2 |
FLUX FOR SOLDERING BY EXTRA QUICK SOLDERS | 2012 |
|
RU2488472C1 |
FLUXING AGENT FOR SOFT SOLDERING | 2006 |
|
RU2347656C2 |
FLUX FOR SOLDERING AND TINNING COPPER WIRE | 2020 |
|
RU2741607C1 |
FLUX FOR LOW TEMPERATURE SOLDERING | 2009 |
|
RU2400340C1 |
Authors
Dates
1996-01-27—Published
1992-07-02—Filed