FIELD: production of titanium dioxide. SUBSTANCE: plasma of oxygen or oxygen-containing gas is prepared and mixed with liquid titanium tetrachloride, ratio of oxygen and titanium tetrachloride being 1.05-1.2 respectively. Temperature of plasma is 2500-3000 C. Thus prepared product having decomposition temperature 1100-1500 C is hardened to temperature being 0.7 of this value. Then this product is cooled in heat exchanger. EFFECT: improves efficiency of method. 1 dwg, 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF PRODUCTION OF TITANIUM DIOXIDE | 1999 | 
 | RU2160230C2 | 
| TITANIUM DIOXIDE MANUFACTURE METHOD | 2002 | 
 | RU2230033C1 | 
| TITANIUM NANOXIDE SYNTHESIS METHOD | 2006 | 
 | RU2321543C1 | 
| INSTALLATION FOR THE SYNTHESIS OF THE TITANIUM DIOXIDE AND THE METHOD FOR THE SYNTHESIS OF THE TITANIUM DIOXIDE | 2005 | 
 | RU2305660C2 | 
| HIGH-DISPERSITY SILICON DIOXIDE POWDER PREPARATION METHOD | 2006 | 
 | RU2314254C1 | 
| PIGMENT TITANIUM DIOXIDE PRODUCTION METHOD | 1998 | 
 | RU2125018C1 | 
| METHOD OF PRODUCING FINE SILICON DIOXIDE POWDER | 2007 | 
 | RU2349546C1 | 
| TITANIUM DIOXIDE PIGMENT PRODUCTION PROCESS | 2006 | 
 | RU2314257C1 | 
| METHOD FOR SYNTHESIS OF NANOSIZE PARTICLES OF TITANIUM DIOXIDE POWDER | 2013 | 
 | RU2547490C2 | 
| ORGANOSILICA PREPARATION METHOD | 2006 | 
 | RU2309120C1 | 
Authors
Dates
1996-04-10—Published
1994-04-11—Filed