FIELD: processing of used rubber, its reclaiming. SUBSTANCE: worn out rubber products are crushed by crusher of the BUZULUK type to obtain particles sizing 1.0-1.5 mm. Added to 100 g of crushed rubber is 10-20 g of synthetic piperylene rubber, mixed at 80-130 C for 10 min, and kept in thermal cabinet to let rubber swell. Then, it is passed through screw extruder. Crushed rubber is introduced into tread rubber compound. Rubber characteristics: tensile strength at 300 C 7.9-8.0 MPa; breaking strength 11.8-12.1 MPa; dynamic tensile endurance at 200 C 3205-3857 cycles. EFFECT: simplified rubber reclaiming process. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING ANHYDRIDE OF ENDO-NORBORNENE-2,3-DICARBOXYLIC ACID | 1992 |
|
RU2032682C1 |
PROCESS OF PRODUCTION OF FLUID PRODUCTS FROM HEAVY PETROLEUM PRODUCTS | 1992 |
|
RU2024578C1 |
PROCESS FOR PREPARING GRANULAR CIS-1,4-POLYISOPRENE | 1994 |
|
RU2076883C1 |
PROCESS FOR PREPARING LIQUID PRODUCTS FROM HEAVY PETROLEUM PRODUCTS | 1992 |
|
RU2024577C1 |
METHOD FOR JOINT PRODUCTION OF ISOPRENE AND 3-METHYLBUTENE-1 | 1992 |
|
RU2030374C1 |
PROCESS FOR PREPARING BOTH ISOPRENE AND 3-METHYLBUTENE-1 | 1992 |
|
RU2032649C1 |
METHOD OF SYNTHESIS OF ENDONORBORNENE-2,3-DICARBOXYLIC ACID ANHYDRIDE | 1992 |
|
RU2021267C1 |
ANTIINFLAMMATORY AGENT | 1994 |
|
RU2118161C1 |
MEDICINAL PREPARATION FOR CURING CEREBRAL ISCHEMIA | 1994 |
|
RU2108095C1 |
ENVIRONMENTALLY APPROPRIATE WOOD-FILLED PLASTIC AND METHOD OF PREPARATION THEREOF | 1995 |
|
RU2081135C1 |
Authors
Dates
1996-06-10—Published
1992-04-03—Filed