FIELD: metallurgy, production of silicon in electric furnaces. SUBSTANCE: method comprises steps of loading and melting charge having ore portion and reduction portion in bath of furnace; using as reduction portion of charge mixture of carbonaceous reducers with next ratio of ingredient (mass %): charcoal 25-35; hard coal 20-25; petroleum coke 30-40; wooden chip 10-15. Inclination angle of generatrix of truncated cone near vertical axis consists 5-12 degrees. EFFECT: enhanced efficiency of the method. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF LOW-GRADE SILICON | 1995 |
|
RU2078035C1 |
METHOD OF SMELTING OF CRYSTALLINE SILICON OR HIGH- SILICON GRADES OF FERROSILICON IN ROTATING ORE-SMELTING ELECTRIC FURNACES | 1994 |
|
RU2057710C1 |
METHOD OF SMELTING CRYSTALLINE SILICON | 1994 |
|
RU2121967C1 |
METHOD OF SILICON PRODUCTION | 1994 |
|
RU2082670C1 |
METHOD OF SMELTING INDUSTRIAL-GRADE SILICON AND HIGH-SILICON SORTS OF FERROSILICON | 1994 |
|
RU2086696C1 |
METHOD FOR TECHNICAL SILICON MELTING | 2016 |
|
RU2649423C1 |
CHARGE FOR CRYSTALLINE SILICON PRODUCING | 1993 |
|
RU2071939C1 |
METHOD OF TECHNICAL SILICON MELTING | 2014 |
|
RU2570153C1 |
METHOD OF HIGHLY SILICEOUS FERROSILICIUM AND TECHNICAL SILICON HEAT | 1994 |
|
RU2068008C1 |
METHOD OF TECHNOLOGICAL SILICON RECEIVING | 2007 |
|
RU2352524C1 |
Authors
Dates
1996-06-27—Published
1994-06-29—Filed