FIELD: production of anticorrosion agents. SUBSTANCE: asphalt from deasphalting process is mixed with still residue of dimethylformaldehyde recovery stage in isoprene production process and sulfuric acid in three steps: first at 120-125 C for 210 min, then at 150 C for 240 min, and finally at 160-180 C for 240 min. Sulfuric acid is evenly entered in the first step with rate 20-35 kg/h per 1 t of reaction mass. Concentration of components is: 75-85 wt % asphalt, 10-15 wt still residue, and sulfuric acid to the balance. EFFECT: enhanced efficiency of process. 4 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING ASMOL | 2010 |
|
RU2443751C1 |
WATERPROOFING MASTIC | 1993 |
|
RU2069224C1 |
MASTIC | 2008 |
|
RU2368637C1 |
INSULATION COMPOSITION AND METHOD FOR PRODUCTION THEREOF | 2012 |
|
RU2508304C1 |
ASMOL PRODUCTION METHOD AND ANTICORROSIVE INSULATING TAPE | 2020 |
|
RU2746727C1 |
MASTIC COMPOSITION AND METHOD OF OBTAINING THEREOF | 2013 |
|
RU2543217C1 |
METHOD FOR RECLAIMING OF RUBBER | 1992 |
|
RU2061710C1 |
INSULATING COMPOSITION | 2013 |
|
RU2539295C1 |
METHOD OF PROCESSING HIGH-MOLECULAR RESIDUES OF PETROLEUM PROCESSING | 1994 |
|
RU2064959C1 |
METHOD OF PRODUCING SULPHUR-BITUMEN BINDER | 2014 |
|
RU2565179C1 |
Authors
Dates
1997-02-27—Published
1994-01-21—Filed