FIELD: chemistry.
SUBSTANCE: composition contains, wt %: oil bitumen or asphalt of propane tar deasphalting of liquid asphalt (PTD) - 86-90, processed absorbent of butadiene and isoprene production - 5-8, sulphuric acid - the remaining part. First oil bitumen or PTD is mixed with absorbent at temperature 100-110°C for 150-180 min, after which sulphuric acid is introduced into reaction mass by dripping at rate 40-50 kg/h at temperature of reaction mass 110-125°C. After that, obtained reaction mass is mixed for 120-150 min at temperature 125-130°C, then temperature is increased to 140°C, after which mixing is continued for 240-300 min. Then temperature of reaction mass is increased to 150°C with mixing for 240 min, after which obtained product is subjected to aging.
EFFECT: obtaining mastic composition with anticorrosion and waterproofing properties, possessing stable exploitation properties.
7 cl, 3 tbl, 2 ex
| Title | Year | Author | Number |
|---|---|---|---|
| INSULATING COMPOSITION | 2013 |
|
RU2539295C1 |
| ASMOL PRODUCTION METHOD AND ANTICORROSIVE INSULATING TAPE | 2020 |
|
RU2746727C1 |
| METHOD OF PRODUCING ASMOL | 2010 |
|
RU2443751C1 |
| METHOD OF PRODUCING INSULATION COMPOSITION (VERSIONS) | 2017 |
|
RU2656486C1 |
| POLYMER-BITUMEN BINDER | 2013 |
|
RU2562496C2 |
| INSULATION COMPOSITION AND METHOD FOR PRODUCTION THEREOF | 2012 |
|
RU2508304C1 |
| COMPOSITE ROOFING MASTIC (VERSIONS) AND A METHOD FOR PRODUCTION THEREOF (VERSIONS) | 2019 |
|
RU2718787C1 |
| METHOD OF PRODUCING ANTICORROSION MASTIC BASED ON ASPHALT-RESIN OLIGOMERS | 2009 |
|
RU2407773C2 |
| METHOD OF PRODUCING ASPHALTITE-CONTAINING ROAD BITUMEN | 2014 |
|
RU2552469C1 |
| ANTI-CORROSION MASTIC MATERIAL | 2008 |
|
RU2384601C2 |
Authors
Dates
2015-02-27—Published
2013-09-27—Filed