FIELD: production of emulsion rubbers. SUBSTANCE: method is carried out by water-emulsion copolymerization of butadiene, acrylonitrile and vinylidene chloride at their mass ratio 10-25:10-20:55-80 respectively. The process takes place in the presence of emulsifier, radical initiator and hydroperoxide of pinane, their quantities being 0.05-0.30 mass parts per 100 mass parts of monomers. Acrylonitrile is fed by steps: 56-85 mass % of acrylonitrile are fed at the beginning of the process, 10-33 mass % are fed when conversion of monomers is 20-30 mass % and 5-11 mass % of acrylonitrile are fed at conversion of monomers 40-55 mass %. Additionally butadiene is fed (its quantity being 5-10 mass parts per 100 mass parts of monomers) when conversion of monomers is 28-32 mass %. Quantity of mentioned above emulsifier is 0.5-1.5 mass % per 100 mass parts of monomers. EFFECT: improves efficiency of the method. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF BUTADIENE-STYRENE(α-METHYL STYRENE) RUBBER BEING MODIFIED BY POLAR MONOMER | 1996 |
|
RU2115664C1 |
METHOD OF SYNTHESIS BUTADIENESTYRENE RUBBER MODIFIED WITH POLAR MONOMER | 1995 |
|
RU2064925C1 |
METHOD FOR PRODUCTION OF COPOLYMER OF BUTADIENE, ACRYLONITRILE AND VINYLYDENE CHLORIDE | 1994 |
|
RU2091403C1 |
METHOD OF PREPARING EMULSION POLYMERIZATION RUBBERS | 1996 |
|
RU2130035C1 |
METHOD OF PREPARING THERMOPLASTIC RUBBER COMPOSITION | 1995 |
|
RU2113445C1 |
THERMOPLASTIC RUBBER COMPOSITION | 1995 |
|
RU2111985C1 |
RUBBER COMPOUND | 1994 |
|
RU2083608C1 |
METHOD OF RUBBER PRODUCTION | 1995 |
|
RU2065451C1 |
METHOD OF PREPARING BUTADIENE-NITRILE RUBBERS | 2000 |
|
RU2167887C1 |
METHOD FOR PRODUCTION OF LATEX OF SYNTHETIC CAOUTCHOUC | 1995 |
|
RU2079513C1 |
Authors
Dates
1997-03-27—Published
1995-08-23—Filed