FIELD: ferrous metallurgy. SUBSTANCE: limestone and iron-containing material mix (24: 1) is supplemented with 35-40% of water based on weight of charge and obtained blend is disintegrated to particle size not greater than 0.08 mm, whereupon blend is charged into rotating tube furnace, burned at torch temperature 1450-1510 C and converted into clots. EFFECT: improved procedure. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF COMPLEX FLUX FOR STEELMAKING PROCESS | 2001 |
|
RU2202627C1 |
METHOD OF PRODUCING IRON-RICH LIME | 2015 |
|
RU2606375C1 |
LINING OF ROTARY TUBULAR FURNACE FOR BURNING OF ORE-LIME MIXTURE | 1991 |
|
RU2037116C1 |
CHARGE FOR THE PRODUCTION OF MAGNESIAN IRON FLUX | 2022 |
|
RU2796485C1 |
MIX MATERIAL FOR PRODUCTION OF MANGANESE-CONTAINING STAFLUX | 2009 |
|
RU2410447C1 |
MIXTURE TO PRODUCE SYNTHETIC LIME-FERRIFERROUS SLAG AND PROCESS OF ITS PREPARATION | 1992 |
|
RU2061060C1 |
METHOD OF PRODUCING FLUX FOR STEEL PRODUCTION | 0 |
|
SU1254021A1 |
LIME-MAGNESIA FLUX AND METHOD FOR ITS PRODUCTION | 2020 |
|
RU2761998C1 |
METHOD OF PRODUCING IRON-RICH DOLOMITE FOR STEEL MAKING | 2018 |
|
RU2693284C1 |
STEEL HIGH-MAGNESIA FLUX AND METHOD OF ITS PRODUCTION (VERSIONS) | 2012 |
|
RU2524878C2 |
Authors
Dates
1997-05-10—Published
1995-06-23—Filed