FIELD: porous materials. SUBSTANCE: method aims at strengthening porous materials, preferably paper, and also leather, fabrics, vegetable and animal specimens (leaves, cockle-shells), and wood by the aid of polymer coating based on di-p-xylylene and its derivatives. Material is treated in vacuum for 5-40 min in sealed chamber with controlled pressure followed by refining material with non-inert gas and subsequently heating di-p- xylylene and/or its derivatives. EFFECT: improved procedure. 2 cl
Title | Year | Author | Number |
---|---|---|---|
DEVICE FOR APPLICATION OF POLY-PARA-XYLYLENE COATING | 1995 |
|
RU2129475C1 |
METHOD OF MODIFYING POLYMER POROUS MATERIAL AND COMPOSITE MATERIAL OBTAINED USING SAID METHOD | 2014 |
|
RU2567886C2 |
METHOD OF BIOLOGICAL CHECKING OF DOCUMENTS IN PROCESS OF THEIR LONG-TIME STORAGE | 1997 |
|
RU2138802C1 |
METHOD AND APPARATUS FOR RESTORATION OF MISSING PARTS OF PAPER SHEETS | 1993 |
|
RU2085644C1 |
METHOD OF NEUTRALIZING ACIDITY OF PAPER | 2003 |
|
RU2243309C1 |
METHOD OF PRODUCING FILMS OF PARYLEN AND ITS DERIVATIVES | 2010 |
|
RU2461429C2 |
METHOD OF PRODUCING COMPOSITE GRADIENT THIN-FILM MATERIAL AND POLYPARAXYLYLENE-BASED MATERIAL | 2010 |
|
RU2461576C2 |
NANOCOMPOSITE POLYMER MATERIAL AND METHOD OF OBTAINING THEREOF | 2012 |
|
RU2523548C2 |
METHOD OF SYNTHESIS OF DI-P-XYLYLENE | 1992 |
|
RU2043323C1 |
METHOD FOR PRODUCING POLYMER MATERIALS CONTAINING PARTICLES OF METALS AND METAL OXIDES WITHIN NANOMETRIC SIZE RANGE | 1996 |
|
RU2106204C1 |
Authors
Dates
1997-05-27—Published
1993-07-02—Filed