FIELD: protective coatings. SUBSTANCE: surface of sheet is first stripped, whereupon aluminium powder is applied followed by, drying, rolling with squeezing, and heat treatment. Rolling is performed in thermostatically controlled mode at 70-80 C with strain whose value is determined from proposed relationship. EFFECT: simplified procedure. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR COATING STEEL STRIP WITH ALUMINUM | 2000 |
|
RU2182191C2 |
METHOD OF STEEL STRIP COATING WITH ANTIFRICTION POWDER MIXTURE | 2001 |
|
RU2208660C1 |
METHOD OF PRODUCING COMPOSITE STEEL-ALUMINIUM LAMINAR MATERIALS | 2012 |
|
RU2501630C1 |
METHOD OF PRODUCING A BIMETALLIC STRIP WITH AN ANTIFRICTION POWDER COATING BASED ON COPPER FOR SLIDING BEARINGS | 2019 |
|
RU2705486C1 |
THERMODIFFUSION ZINC-PLATING METHOD | 1998 |
|
RU2147046C1 |
POWDER FOR GAS-THERMIC COATINGS | 1991 |
|
RU2016914C1 |
PROCESS OF THERMAL-DIFFUSION TREATMENT OF ARTICLES MADE OF METALS AND ALLOYS | 2001 |
|
RU2221898C2 |
BORONIZING MELT COMPOSITION | 2001 |
|
RU2215060C2 |
METHOD OF MAKING HOT ROLLED STRIP OF MAGNETIC ALLOYS ON BASE OF INTERMETALIC COMPOUNDS; INCLUDING RARE-EARTH ELEMENTS | 1993 |
|
RU2061562C1 |
ALLOY ON THE BASE OF FERRUM FOR POWDER GAS THERMIC COATINGS | 1995 |
|
RU2094522C1 |
Authors
Dates
1997-06-20—Published
1994-09-08—Filed