FIELD: powder metallurgy. SUBSTANCE: method involves preparing burden; manufacturing billets with shape close to that of ready part; performing homogenizing annealing, mechanical working and quenching. Burden is completed with 5-12% of hardening powder and 1-1.5% of carbon. Billets are manufactured by pressing. Homogenizing annealing is conducted at temperature of 1,130-1,180 C for 2-4 hours and is combined with copper infiltration. Quenching is effectuated from temperature of 850-1,050 C. EFFECT: simplified method and improved quality by high abrasive resistance. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING POWDERED CONCENTRATIONALLY-HETEROGENEOUS TRANSFORMATION-INDUCED PLASTICITY STEEL | 1996 |
|
RU2088375C1 |
METHOD FOR MAKING POWDER ARTICLES | 1997 |
|
RU2118584C1 |
METHOD OF JOINING PARTS MADE FROM POWDER MATERIALS | 1997 |
|
RU2120352C1 |
METHOD OF DIAMOND TOOL MANUFACTURE | 1998 |
|
RU2148490C1 |
METHOD OF MANUFACTURING PARTS FROM POWDER MATERIALS | 1994 |
|
RU2080210C1 |
METHOD OF MANUFACTURING PHOSPHORUS STEEL | 1998 |
|
RU2132254C1 |
METHOD OF MANUFACTURING PARTS FROM BRONZE-STEEL PSEUDOALLOY | 1999 |
|
RU2163270C2 |
METHOD OF PRODUCTION OF SUPERFINE COMPOSITE POWDER BASED ON ZIRCONIUM DIOXIDE | 1996 |
|
RU2136443C1 |
METHOD OF PRODUCTION OF ULTRAFINE POWDER OF ZIRCONIUM DIOXIDE WITH COATING | 1995 |
|
RU2087254C1 |
METHOD FOR PRODUCING METALLOFULLERITE | 2000 |
|
RU2178350C2 |
Authors
Dates
1997-06-27—Published
1993-12-27—Filed