FIELD: chemical technology. SUBSTANCE: process of butadiene-1,3 polymerization is carried out for two stages. At the first stage n-butyllithium (12-30 mole per 1 t monomer) and modifying addition taken from the group: diethylene glycol dimethyl ether, diethylene glycol divinyl ether, tetramethylethylenediamine, permethylated polyethylenepolyamines, dipiperidineethane (mole ratio to n-butyllithium = 0.1-5.0) were added to charge containing monomer at the parent concentration 10-20 wt.-%. Process is carried out at 20-45 C up to monomer conversion 95%, not less. At the second stage divinylbenzene is added (mole ratio to n-butyllithium = 0.1-0.5), kept for at least 16 min followed by additional addition of butadiene-1,3 as the charge at the same parent concentration of monomer (mass ratio to butadiene-1,3 = 0.8-1.2) and process is carried out at 45-80 C up to conversion 95%, not less. Method is used for synthesis of high-molecular polybutadiene that can be used in rubber industry. EFFECT: improved properties of 1,2-polybutadiene. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS FOR PREPARING LOW MOLECULAR WEIGHT 1,2-POLYBUTADIENE | 1995 |
|
RU2082722C1 |
PROCESS FOR PREPARING 1,2-POLYBUTADIENE | 1994 |
|
RU2080329C1 |
PROCESS FOR PREPARING 1,2-POLYBUTADIENE | 1993 |
|
RU2054010C1 |
METHOD OF PREPARING BUTADIENE-STYRENE BLOCK COPOLYMER | 1998 |
|
RU2140934C1 |
METHOD OF PREPARING 1,2-POLYBUTADIENE | 1998 |
|
RU2134697C1 |
METHOD OF PREPARING LOW-MOLECULAR 1,2-POLYBUTADIENE | 1998 |
|
RU2142474C1 |
PROCESS FOR PREPARING POLYBUTADIENE | 1994 |
|
RU2080328C1 |
METHOD OF POLYBUTADIENE SYNTHESIS | 1993 |
|
RU2028310C1 |
METHOD OF PRODUCING MODIFIED POLYBUTADIENE | 1997 |
|
RU2128669C1 |
METHOD OF SYNTHESIS OF BUTADIENE-STYRENE RUBBER | 2001 |
|
RU2200740C1 |
Authors
Dates
1997-07-10—Published
1995-02-17—Filed