FIELD: metal working. SUBSTANCE: method consists in vacuum heating to 1070-1180 C with specified rate, aging for 10-15 min, cooling with rate 0.9-1.1 C/s to 600-700 C, and drawing without depressurization of furnace at 180-580 C in vacuum up to I0-5 mm Hg. EFFECT: optimized conditions of procedure. 9 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR TREATING TOOL MADE FROM QUICK-CUTTING STEEL | 1992 |
|
RU2041280C1 |
PORTABLE VACUUM FURNACE FOR CHEMICAL-THERMAL TREATMENT OF SMALL-SIZE TOOL AND STRUCTURAL PARTS | 1992 |
|
RU2006773C1 |
STAINLESS STEEL MEDICAL TAIL INSTRUMENT PRODUCTION METHOD | 1992 |
|
RU2034046C1 |
METHOD OF HEAT TREATMENT OF FINE-BLADE TOOLS OF STAINLESS STEEL AGING IN MARTENSITE MODE | 1992 |
|
RU2085599C1 |
METHOD OF HEAT TREATMENT OF RESILIENT STEEL AND ALLOY MEMBERS | 1993 |
|
RU2093589C1 |
METHOD OF TREATMENT OF PRECISION PARTS FROM TITANIUM ALLOYS | 1993 |
|
RU2075536C1 |
METHOD FOR TREATING PARTS OF MICROELECTRICAL VALVES MADE OF SPECIAL STEEL | 1994 |
|
RU2090628C1 |
METHOD OF PRESSURE-TREATING DIE STEEL MOLDS | 0 |
|
SU1786184A1 |
METHOD OF HARDENING OF STEEL PRODUCTS | 0 |
|
SU1713976A1 |
PROCESS FOR MANUFACTURING STAINLESS STEEL MEDICAL END TOOLS | 1992 |
|
RU2031185C1 |