FIELD: electrical engineering. SUBSTANCE: cathode material has the following composition, mass percent: iron disulfide - 57-80; lithium hydroxide - 0.7-17; magnesium oxide - 8.3-12; saline electrolyte - 11-14. EFFECT: improved stability of current supply characteristics at start of discharge. 2 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| ELEMENT OF THERMALLY ACTIVATED CHEMICAL CURRENT SOURCE | 2021 |
|
RU2768252C1 |
| ACTIVE MATERIAL OF CHEMICAL CURRENT SOURCE PLATE | 1988 |
|
RU2154326C2 |
| METHOD OF MAKING CATHODE MASS FOR THERMAL CHEMICAL CURRENT SOURCE | 2024 |
|
RU2824758C1 |
| CYLINDRICAL CHEMICAL SOURCE OF ELECTRIC ENERGY OF AIR-AND-ZINC | 1992 |
|
RU2040833C1 |
| ELECTROLYTE MASS AND METHOD OF MAKING ELECTROLYTE FOR THERMAL CHEMICAL SOURCES OF CURRENT | 2019 |
|
RU2732080C1 |
| ELECTROCHEMICAL THERMAL BATTERY | 1987 |
|
RU2091918C1 |
| METHOD FOR PRODUCING ELECTROLYTE MIXTURE FOR THERMAL CURRENT SUPPLY | 1986 |
|
SU1840220A1 |
| THERMAL BATTERY | 2020 |
|
RU2744416C1 |
| ELECTROLYTIC DEPOSITION OF LITHIATED TRANSITION METAL OXIDES, WHEN USING INITIAL PRECURSORS WITH LOW PURITY DEGREE | 2019 |
|
RU2784167C2 |
| IMPROVED ELECTROCHEMICAL ELEMENTS FOR USE IN HIGH-ENERGY CURRENT SOURCE | 2018 |
|
RU2786089C2 |
Authors
Dates
1997-10-20—Published
1991-02-06—Filed