FIELD: chemical technology. SUBSTANCE: method involves mixing the technical zinc oxide with water and zinc monophosphate solution at weight ratio ZnO : water : zinc monophosphate solution = 1:(1-4):(3-11) followed by addition of nitric acid. Before nitric acid addition sodium chlorate solution is added at amount 0.25-0.45 weight % (as measured for NaClO3). Nitric acid is added at the rate 30-70 kg/min. Invention can be used for making phosphatic concentrates. EFFECT: increased stability of concentrates, decreased time for composition correction and preparing, decreased cost. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ZINC-NITRATE-PHOSPHATE CONCENTRATE PRODUCING | 1993 |
|
RU2094368C1 |
METHOD OF PREPARING ZINC NITRATE-PHOSPHATE CONCENTRATE | 1994 |
|
RU2107025C1 |
METHOD OF PREPARING SOLUTION FOR ZINC NITRATE/PHOSPHATE CONCENTRATE | 1994 |
|
RU2106300C1 |
METHOD OF ZINC-NITRATE-PHOSPHATE CONCENTRATE PRODUCING | 1994 |
|
RU2100275C1 |
METHOD OF ZINC-NITRATE-PHOSPHATE CONCENTRATE PRODUCING | 1994 |
|
RU2094369C1 |
METHOD OF PRODUCTION OF PHOSPHATING CONCENTRATE | 2001 |
|
RU2195426C2 |
SOLUTION FOR PHOSPHATING | 1993 |
|
RU2065892C1 |
METHOD FOR PRODUCTION OF ZINC-NITRATE-PHOSPHATE CONCENTRATE | 1996 |
|
RU2111919C1 |
SOLUTION FOR SIMULTANEOUS DEFATTING AND PHOSPHATING | 1993 |
|
RU2063476C1 |
METHOD FOR PRODUCTION OF ZINC NITRATE-PHOSPHATE CONCENTRATE | 1996 |
|
RU2110476C1 |
Authors
Dates
1997-10-27—Published
1993-11-09—Filed