FIELD: inorganic chemistry. SUBSTANCE: method involves mixing zinc oxide, water and solution of zinc monophosphate at weight ratio = 1:(1-4):(3-11), respectively, followed by addition of nitric acid and solution of calcium nitrate at amount 0.1-5.0 weight % (as measured for calcium). Temperature of reaction mixture is 50-60 C. Nitric acid is added at the rate 70-120 kg/min. The proposed concentrate is used in metallurgy and other industries. EFFECT: increased stability of concentrate, simplified method. 4 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD FOR PRODUCTION OF ZINC NITRATE-PHOSPHATE CONCENTRATE | 1996 |
|
RU2110476C1 |
| METHOD FOR PRODUCTION OF ZINC-NITRATE-PHOSPHATE CONCENTRATE | 1996 |
|
RU2111919C1 |
| METHOD OF PREPARING ZINC NITRATE PHOSPHONATE CONCENTRATE | 1995 |
|
RU2115618C1 |
| METHOD OF ZINC-NITRATE-PHOSPHATE CONCENTRATE PRODUCING | 1994 |
|
RU2094369C1 |
| METHOD OF PRODUCTION OF PHOSPHATING CONCENTRATE | 2001 |
|
RU2195426C2 |
| METHOD OF PREPARING SOLUTION FOR ZINC NITRATE/PHOSPHATE CONCENTRATE | 1994 |
|
RU2106300C1 |
| METHOD OF ZINC-NITRATE-PHOSPHATE CONCENTRATE PRODUCING | 1993 |
|
RU2094368C1 |
| METHOD OF PRODUCING ZINC NITRATE | 1996 |
|
RU2108285C1 |
| SOLUTION FOR PHOSPHATATION OF METAL SURFACE | 1996 |
|
RU2111282C1 |
| METHOD OF RECOVERING ZINC FROM ZINC-CONTAINING WASTE | 1996 |
|
RU2103387C1 |
Authors
Dates
1997-12-27—Published
1994-07-25—Filed