FIELD: waste disposal. SUBSTANCE: zinc-containing materials, in particular, zinc cuttings, without preliminary crushing, are placed into water and to the mixture obtained, phosphoric acid is added under stirring at zinc/phosphorus pentoxide/water ratio (0.94-1):(3.15-3.88):(1.56- 3.02). Zinc is recovered at 20-45 C. EFFECT: facilitated recovery procedure. 3 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF ZINC-NITRATE-PHOSPHATE CONCENTRATE | 1996 |
|
RU2111919C1 |
METHOD OF ZINC-NITRATE-PHOSPHATE CONCENTRATE PRODUCING | 1993 |
|
RU2094368C1 |
METHOD OF ZINC-NITRATE-PHOSPHATE CONCENTRATE PRODUCING | 1994 |
|
RU2094369C1 |
METHOD FOR EXTRACTING ZINC FROM ZINC CONTAINING WASTE | 2016 |
|
RU2661323C2 |
METHOD FOR PRODUCTION OF ZINC NITRATE-PHOSPHATE CONCENTRATE | 1996 |
|
RU2110476C1 |
METHOD OF ZINC-NITRATE-PHOSPHATE CONCENTRATE PRODUCING | 1994 |
|
RU2100275C1 |
METHOD OF PRODUCTION OF PHOSPHATING CONCENTRATE | 2001 |
|
RU2195426C2 |
METHOD OF PHOSPHATIZING METALLIC SURFACE | 1996 |
|
RU2113541C1 |
SOLUTION FOR PHOSPHATATION OF METAL SURFACE | 1996 |
|
RU2111282C1 |
METHOD OF PREPARING ZINC NITRATE-PHOSPHATE CONCENTRATE | 2008 |
|
RU2380458C1 |
Authors
Dates
1998-01-27—Published
1996-06-18—Filed