FIELD: metallurgy. SUBSTANCE: powder is fed from one nozzle into head part of laser spot following movement of article. Powder form other nozzle is fed into central and tail parts of laser spot in opposition to movement of article. EFFECT: increased coefficient of usage of powder, decreased ratio of height of surfaced bead to width to prevent appearance of incomplete fusion on sides of bead. 1 dwg, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
DEVICE FOR LASER HARD-FACING | 1996 |
|
RU2104135C1 |
METHOD OF FOUR-SUCCESSFUL GAS-POWDER LASER WELDING WITH REGULATION OF FLOW OF POWDER | 2016 |
|
RU2660499C2 |
LASER MANUFACTURING INSTALLATION | 1992 |
|
RU2049629C1 |
LASER TREATMENT OBJECTIVE | 1992 |
|
RU2049632C1 |
METHOD FOR LASER TREATMENT OF SPLINE GROOVE SIDE SURFACES | 1993 |
|
RU2050240C1 |
METHOD OF POWDER LASER SURFACING OF ANGLE PIECES | 1997 |
|
RU2123418C1 |
INTERFERENCE MIRROR | 1995 |
|
RU2097802C1 |
LIGHT SPLITTING INTERFERENCE COATING | 1994 |
|
RU2097800C1 |
METHOD OF NONDESTRUCTIVE TESTING OF SURFACE | 1994 |
|
RU2083973C1 |
DEVICE FOR NON-DESTRUCTIVE TESTING OF OBJECT SURFACE | 1994 |
|
RU2083974C1 |
Authors
Dates
1997-12-27—Published
1996-01-04—Filed