FIELD: power engineering. SUBSTANCE: method involves building up iron-chromium-base material on outer shell section edges to be welded; assembling and soldering shells; providing mechanical working of edges to be welded, with built-up material being completely removed; welding outer shell; subjecting obtained telescopic joint to thermal treatment by gradual heating to 750 C plus and minus 10 C; holding for 50-70 min. Method allows hermetically sealed construction with high strength characteristics and welded joints free of cracks to be obtained. EFFECT: increased efficiency, simplified method and improved quality of joints.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURE OF SOLDERED TELESCOPIC CONSTRUCTION | 1996 |
|
RU2106230C1 |
PROCESS OF SOLDERING OF TELESCOPIC STRUCTURES | 1996 |
|
RU2106941C1 |
METHOD OF SOLDERING OF TELESCOPIC STRUCTURES | 1996 |
|
RU2094190C1 |
METHOD OF SURFACING BUTT JOINED EDGES OF WORKPIECES | 1993 |
|
RU2063313C1 |
METHOD OF MAKING SOLDERED TELESCOPIC STRUCTURES | 1996 |
|
RU2109606C1 |
METHOD OF SOLDERING TELESCOPIC STRUCTURES | 1996 |
|
RU2096143C1 |
PROCESS OF SOLDERING OF TELESCOPIC STRUCTURES | 1996 |
|
RU2106942C1 |
SOLDER FOR PARTS SOLDERING | 1996 |
|
RU2129482C1 |
SOLDER FOR SOLDERING OF COPPER-STEEL ARTICLES | 1996 |
|
RU2129063C1 |
SOLDER FOR SOLDERING OF STEEL ARTICLES | 1996 |
|
RU2129062C1 |
Authors
Dates
1998-03-10—Published
1996-09-05—Filed