FIELD: manufacture of building materials. SUBSTANCE: method includes crushing clayey rock, adding 6-10 wt % of oil sludge with 3-30 wt % water preheated to 80-95 C, and additional water. Amount of the latter is determined from the equation: A=X-(Y+0.01Cg) where X is optimum content of water in clayey batch (16-20 wt %); Y content of water in clayey rock, wt %; C amount of oil sludge added, wt %; and g content of water in oil sludge, wt %. Afterwards granules are shaped, dried, roasted, and cooled. EFFECT: decreased apparent density and increased strength. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING HYDROINSULATING ROOFING MATERIAL | 1999 |
|
RU2175661C2 |
HYDROINSULATING ROOFING MATERIAL | 1999 |
|
RU2176653C2 |
CRUDE MIXTURE FOR PRODUCING EXPANDED CLAY | 2011 |
|
RU2467966C1 |
METHOD FOR PREPARING ASPHALT-CONCRETE MIXTURE | 1996 |
|
RU2110496C1 |
RAW MIXTURE FOR BRICK MAKING | 1996 |
|
RU2114086C1 |
ORGANIC FERTILIZER | 2000 |
|
RU2210557C2 |
METHOD OF PREPARING EXPANDED CLAY | 2008 |
|
RU2397963C2 |
ROAD PAVEMENT LAYING METHOD | 2000 |
|
RU2179609C1 |
METHOD FOR PREPARING ORGANIC FERTILIZER | 2000 |
|
RU2216527C2 |
REAGENT FOR REMOVING WATER WELL SEDIMENTATION | 1993 |
|
RU2092683C1 |
Authors
Dates
1998-06-10—Published
1996-10-15—Filed