FIELD: manufacture of building materials. SUBSTANCE: suspension of silica-containing amorphous material with particle size (0.1-0.1) •10-6 M in sodium hydroxide solution with solid to liquid phase ratio 1:(2.0-5.32) is subjected to hydrothermal treatment at atmosphere pressure and temperature 70-75 C for 8-60 min. EFFECT: reduced duration of process and its temperature, and expanded range of liquid glass properties. 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF LIQUID GLASS PRODUCTION | 1995 | 
 | RU2085489C1 | 
| METHOD PREPARING LIQUID GLASS | 1998 | 
 | RU2135410C1 | 
| METHOD OF PRODUCTION OF HIGH-MODULUS WATER GLASS | 1998 | 
 | RU2142411C1 | 
| METHOD OF WATER GLASS PRODUCTION | 1999 | 
 | RU2181691C2 | 
| METHOD FOR PRODUCTION SPECIAL-DESTINATION LIQUID GLASS | 2000 | 
 | RU2171222C1 | 
| METHOD OF MAKING LIQUID GLASS | 1999 | 
 | RU2172295C1 | 
| METHOD FOR PRODUCTION SPECIAL-DESTINATION LIQUID GLASS | 1999 | 
 | RU2171223C1 | 
| METHOD OF WATER GLASS PRODUCTION | 1999 | 
 | RU2181692C2 | 
| METHOD OF PREPARING GRANULAR HEAT-INSULATING MATERIAL | 2000 | 
 | RU2177921C2 | 
| METHOD OF PREPARING HIGH-MODULUS LIQUID GLASS | 2000 | 
 | RU2171221C1 | 
Authors
Dates
1999-05-10—Published
1998-03-25—Filed