FIELD: building materials; manufacture of thin-walled elements. SUBSTANCE: lengths of nonmetallic fiber (up to 4% by volume) are introduced into cement-sand-water mixture in process of mixing. Part of prepared fiber-concrete mixture is placed in mould and vibrated. Mixture spreads under effect of thixotropy in layer of 2-3 mm thick. Then glass roving preliminarily impregnated with cement grout modified with additives is placed on under layer. This done, mould is filled with fiber-concrete mixture up to the top and vibrated again. EFFECT: production material of low specific amount of metal and high strength. 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MAKING GLASS ROVING IN HARDENING CEMENT STONE | 1996 |
|
RU2115633C1 |
FIBER-REINFORCED CONCRETE MIXTURE | 2014 |
|
RU2575658C1 |
CRUDE MIXTURE FOR LIGHT FIBRE CONCRETE | 2019 |
|
RU2734485C1 |
METHOD FOR PREPARATION OF MODIFIED FIBROUS CONCRETE MIX AND MODIFIED FIBROUS CONCRETE MIX | 2009 |
|
RU2397069C1 |
FINE-GRAINED CEMENT CONCRETE BASED ON MODIFIED BASALT FIBRE | 2013 |
|
RU2530812C1 |
METHOD OF MAKING DECORATIVE REINFORCED CONCRETE ARTICLES | 2011 |
|
RU2481946C2 |
METHOD FOR CONSTRUCTION OF THIN-WALLED MONOLITHIC SHELLS | 2022 |
|
RU2795782C1 |
MIXTURE FOR PRODUCING FINE-GRAINED STEEL FIBRE CONCRETE BASED ON QUARTZITE SANDSTONE GRINDING SCREENINGS | 2011 |
|
RU2467972C1 |
TECHNIQUE OF CASTING CONCRETE ON AIRFIELD AND ROAD PAVEMENT | 2001 |
|
RU2206657C1 |
0 |
|
SU1778100A1 |
Authors
Dates
1999-05-20—Published
1997-07-24—Filed