FIELD: wood-working industry, in particular, production of wood bars from low-value trees with predetermined qualities. SUBSTANCE: method involves impregnating wood with carbamide solution containing urotropin in an amount of 6-10% by weight of dried carbamide, with pH value of solution being within the range of 6.4-6.5, with following drying under pressure and at temperature of 90-120 C. Method allows wood with volumetric swelling rate not in excess of 25% to be obtained. EFFECT: simplified method, increased efficiency and improved quality of wood bars. 1 dwg, 2 ex
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD FOR PRODUCTION OF MODIFIED WOOD | 2001 | 
 | RU2229377C2 | 
| METHOD OF PRODUCING MODIFIED WOOD | 2018 | 
 | RU2710171C1 | 
| METHOD OF PRODUCING MODIFIED TIMBER | 2008 | 
 | RU2401195C2 | 
| METHOD OF PRODUCING ACETYLATED WOOD | 2007 | 
 | RU2391202C1 | 
| METHOD OF PRODUCING MODIFIED WOOD | 2019 | 
 | RU2712521C1 | 
| METHOD OF TIMBER MODIFICATION | 2011 | 
 | RU2476311C1 | 
| METHOD FOR PRODUCTION OF WOODEN SUPPORTS OF ELECTRICITY TRANSMISSION LINES | 2021 | 
 | RU2777903C1 | 
| METHOD OF PRODUCING MODIFIED WOOD | 2014 | 
 | RU2605752C2 | 
| METHOD OF PRODUCING WOOD WITH MODIFIED TEXTURE | 2019 | 
 | RU2726556C1 | 
| COMPOSITION FOR PREPARING SOLUTION FOR WOOD IMPREGNATION, SOLUTION FOR WOOD IMPREGNATION AND METHOD FOR USING THIS SOLUTION | 2021 | 
 | RU2771676C1 | 
Authors
Dates
1999-06-10—Published
1997-11-19—Filed