FIELD: manufacture of high-strength oil application pipes resistant to sulfide corrosion cracking. SUBSTANCE: method includes pipe rolling at 850-930 C, cooling from temperature of rolling end in water for 1-2 s down to temperature of 630-670 C, repeated heating up to 780-830 C with subsequent cooling in water and tempering at 650-720 C. EFFECT: higher strength properties of pipes and their resistance to sulfide corrosion cracking. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS OF MANUFACTURE OF PIPES FROM CARBON STEEL | 1998 |
|
RU2132396C1 |
METHOD OF PIPE MANUFACTURE | 1997 |
|
RU2110588C1 |
METHOD OF MANUFACTURING PIPES FROM CARBON AND LOW-ALLOYED STEELS | 1999 |
|
RU2153011C1 |
METHOD OF PIPE HEAT TREATMENT | 1997 |
|
RU2112050C1 |
METHOD OF HIGH-HEAT TREATMENT OF PIPES | 2003 |
|
RU2230802C1 |
METHOD OF HEAT TREATMENT OF PIPES | 1996 |
|
RU2085596C1 |
LOW-CARBON MANGANESE STEELS PIPES HEAT TREATMENT METHOD | 1994 |
|
RU2048542C1 |
METHOD OF HEAT TREATMENT OF PIPES | 1996 |
|
RU2086670C1 |
METHOD FOR MANUFACTURE OF STRIPS FROM LOW-ALLOY NIOBIUM-VANADIUM STEEL | 2000 |
|
RU2195504C2 |
METHOD OF HEAT TREATMENT OF PIPES MADE OF CARBON AND LOW-ALLOYED STEELS | 1997 |
|
RU2112052C1 |
Authors
Dates
1999-06-20—Published
1998-06-22—Filed