FIELD: trolley buses, trams, miscellaneous pieces of rolling stock. SUBSTANCE: powdered graphite is introduced in aluminum-alloy slitter in the amount of 0.5-10.0 mass percent as reinforcing phase of metal matrix. Proportion of ingredients is as follows, mass percent: silicon - 0.8-22.0; zinc - г12.0; iron - 0.3-3.5; magnesium - г2.0; other impurities - <6.0; aluminum - the rest. EFFECT: improved performance characteristics. 2 ex
Title | Year | Author | Number |
---|---|---|---|
CONTACT INSERT FOR TROLLEYBUS CURRENT COLLECTOR | 1997 |
|
RU2141413C1 |
METHOD FOR MAKING CASTING WITH ENHANCED WEAR-RESISTANCE | 2000 |
|
RU2192938C2 |
METHOD FOR PRODUCING CAST PIECES OF BLAST-FURNACE CAST IRON | 2005 |
|
RU2300441C1 |
OXYGEN CONVERTER TUYERE TIP | 2006 |
|
RU2316601C2 |
CURRENT COLLECTOR CONTACT SLIPPER | 1999 |
|
RU2156704C1 |
METHOD OF MANUFACTURE OF ROLLS | 1992 |
|
RU2009016C1 |
METHOD OF MANUFACTURE OF PISTON FOR INTERNAL COMBUSTION ENGINE | 2006 |
|
RU2318126C1 |
METHOD OF MANUFACTURING BULK CATALYST CARRIER WITH HONEYCOMB STRUCTURE | 1992 |
|
RU2104781C1 |
CASTING MOLD FOR PRODUCING ANNULAR INGOTS | 1997 |
|
RU2108200C1 |
METHOD FOR PRODUCING INGOTS BY SQUEEZING COMBINED WITH CRYSTALLIZATION UNDER PRESSURE | 1990 |
|
RU2048253C1 |
Authors
Dates
1999-09-10—Published
1997-12-16—Filed