FIELD: manufacture of building materials; finishing external and internal surfaces of buildings. SUBSTANCE: method includes application of mixture of water glass mixed preliminarily with silica and pigment on surface of mixer followed by hardening in the course of application at supply of air at temperature of 58 to 79 C, after which final hardening of mixture is performed at temperature of 80 to 150 C. Then decorative filler is rubbed through sieve. Application of above-mentioned mixture is performed for each fraction separately. EFFECT: enhanced water and alkaline resistance of filler.