FIELD: ferrous metallurgy, preparation of metal-bearing burden for melting of steel and alloys in arc electric furnaces. SUBSTANCE: burden blank is prepared by loading of solid filling agents into charging boxes of casting conveyer and by pouring liquid iron-carrying alloy on to them in two steps. Temperature of poured alloy is 1381-1450 C. Pigs removed from charging boxes are tumbled. Tumbling barrel is positioned casting machine between conveyer and container for collection and transportation of blanks. Burden composed of iron- carrying material, ground quicklime in the amount of 1.0-10.0 per cent by mass and carbon-carrying material in the amount of 0.5-5.0 per cent by mass is used to prepare pellets employed as filling agents in burden blank. EFFECT: stability of composition of burden blank and of carbon content in melt. 12 cl, 1 dwg, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MAKING SEMIFINISHED PRODUCT FOR METALLURGICAL CONVERSION | 1999 |
|
RU2146181C1 |
FILLER FOR MATERIAL DESTINED FOR METALLURGICAL PRODUCTION AND METHOD FOR PREPARING FILLER FOR MATERIAL DESTINED FOR METALLURGICAL PRODUCTION | 2000 |
|
RU2170270C1 |
POLYHEDRAL CHARGE BLANK, ITS CASTING MOLD AND METAL CASTING METHOD | 1993 |
|
RU2032752C1 |
METHOD OF PREPARING CHARGE MATERIAL FOR METALLURGICAL CONVERSION | 1999 |
|
RU2149190C1 |
METHOD OF PIG IRON SMELTING IN ARC FURNACE | 1998 |
|
RU2142516C1 |
METHOD OF MAKING SEMIFINISHED PRODUCTS FOR METALLURGICAL CONVERSION | 1992 |
|
RU2031965C1 |
METHOD OF CAST IRON SMELTING IN BLAST FURNACE | 1999 |
|
RU2157413C1 |
CAST IRON AND A METHOD OF SMELTING THEREOF IN BLAST FURNACE | 1998 |
|
RU2128239C1 |
CAST IRON | 1999 |
|
RU2149913C1 |
METHOD OF PRODUCTION OF CHARGE STOCK | 1995 |
|
RU2086342C1 |
Authors
Dates
2000-04-27—Published
1998-08-13—Filed