FIELD: building materials. SUBSTANCE: invention relates to finishing and restoration works making. Phosphate material based on loam and phosphoric acid has iron-containing waste of metallurgic production at the following ratio of components, wt.-%: loam 71-74; iron-containing waste of metallurgic production at residue on sieve N 008 5-7% 7-11; ortho-phosphoric acid of specific gravity 1.24-1.25 g/cm3 - the rest. Invention provides replacing expensive ferrous (II) oxide by iron-containing waste of metallurgical production. EFFECT: waterproof phosphate material making, decreased cost. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
CLAY-PHOSPHATE MATERIAL | 2002 |
|
RU2232146C1 |
CLAY-PHOSPHATE MATERIAL | 2009 |
|
RU2396229C1 |
CLAY-PHOSPHATE MATERIAL | 2009 |
|
RU2398750C1 |
CLAY-PHOSPHATE MATERIAL | 2009 |
|
RU2394002C1 |
CLAY-PHOSPHATE MATERIAL | 2009 |
|
RU2396230C1 |
CLAY-PHOSPHATE MATERIAL | 2002 |
|
RU2232147C1 |
CLAY PHOSPHATE MATERIAL | 2007 |
|
RU2351564C1 |
CLAY-PHOSPHATE MATERIAL | 2005 |
|
RU2285682C1 |
CLAY-PHOSPHATE MATERIAL | 1998 |
|
RU2138532C1 |
CLAY-PHOSPHATE MATERIAL | 2007 |
|
RU2336242C1 |
Authors
Dates
2000-05-10—Published
1998-06-08—Filed