FIELD: metal coatings. SUBSTANCE: process involves preliminarily saturation of nickel at 350-500 C during 5 to 30 min and saturation with boron at 600 to 950 C. The former is conducted in composition containing, wt %: nickel oxide 0.02-0.5, boron carbide 5-35, ammonium chloride 0.005-0.2, sodium tetrafluoroborate 0.01-0.1, and corundum - the balance. EFFECT: enabled preparation of high-quality boron-nickel layers 90-120 mcm thick with microhardness 14000 MPa. 1 tbl